Fatigue strength

Updated on: 11.11.2024

Fatigue strength indicates how long a material withstands cyclic loading without significant fatigue or failure. It is also referred to as endurance limit and can be determined in a fatigue test. The relationship between stress and the service life of a material can be illustrated in various diagrams, for example by means of the S-N curve (Wöhler curve). Fatigue strength is a decisive factor in the selection of materials in industries such as mechanical engineering and the automotive industry.

Diagrams for fatigue strength

In connection with fatigue strength there are various diagrams, each of which shows different aspects. The S-N diagram shows the results of the fatigue test according to August Wöhler.

 

The S-N diagram assumes a specific mean stress. In dynamically loaded materials, however, the mean stress changes over time. This relationship is shown in the Smith and Haigh diagrams.

Fatigue test (Wöhler curve)

The fatigue test is used to determine the fatigue strength. The test set-up provides for testing different specimens at different load levels. Each test is repeated until the material fails according to a previously defined criterion (for example when cracks form or at fracture).

 

The Wöhler curve in the S-N diagram shows the results of the fatigue test in the form of the nominal stress amplitude Sa. The mean stress is the mean of the maximum stress applied in the test, the upper stress So, and the minimum stress applied, the lower stress Su. This gives the following formula:

 

Wöhler curve

Smith diagram

The Smith diagram shows the relationships between mean stress, amplitude, stress and fatigue strength. To simplify the complex calculations, Goodman lines are used. The Smith diagram then shows the upper stress So and lower stress Su permissible for fatigue strength in each case as a function of the mean stress Sm.

 

Smith diagram

Haigh diagram

The Haigh diagram shows the fatigue-resistant stress amplitude plotted against the mean stress. Straight lines through the origin also help to read off the stress ratios from the value pairs of stress amplitude and mean stress. The Goodman line is used for simplification. The fatigue strength range lies below it. The mean stress sensitivity can be determined from the slope of the Goodman line.

Haigh diagram

Factors influencing fatigue strength

The individual fatigue strength depends on the one hand on the nature of the material and on the other on external influences such as the type of loading, corrosion and temperature. These aspects interact with each other. One of the most important influencing factors is residual stress.

Residual stress

Residual stresses arise in a material due to various factors and occur in almost all phases of material processing and use. Depending on the type of stress, there are different effects on fatigue strength. Compressive residual stresses have a positive influence, while tensile residual stresses reduce fatigue strength.

 

The decisive factor is the respective influence on the mean stress, which in turn is decisive for fatigue strength. Weld seams, for example, are under high tensile stresses. Manufacturing processes such as finish rolling can introduce compressive residual stresses in order to increase fatigue strength.

Component properties

In addition to residual stress, a number of other component properties influence fatigue strength.

Tensile strengthFatigue strength is proportional to the tensile strength of the
material. This means that as tensile strength increases, so does
fatigue strength.
DuctilityHigh ductility has a positive effect on the
mean stress sensitivity and thus on fatigue strength.
RoughnessHigh ductility has a positive effect on the
mean stress sensitivity and thus on fatigue strength.
Component sizeComponent size influences technological aspects
such as the surface layer thickness or the surface layer strength. In addition, the volume and the surface subjected to the load
also change with size. This influences the statistical distribution of defects.
Furthermore, larger components, under otherwise identical conditions, exhibit a
lower stress gradient. This reduces the supporting effect of the surrounding material and thus also the fatigue strength.
OtherComponent size influences technological aspects
such as the surface layer thickness or the surface layer strength. In addition, the volume and the surface subjected to the load
also change with size. This influences the
statistical distribution of defects.
Furthermore, larger components, under otherwise identical conditions, exhibit a
lower stress gradient. This reduces the supporting effect of the surrounding material and thus also the fatigue strength.

External influencing factors

External influencing factors and the intended use of the workpiece must also be taken into account with regard to fatigue strength.

Type of loadingLoading in the form of shear stress requires a higher fatigue strength than loading that produces normal stress.
Load peaksIf load peaks occur above the fatigue strength of a material, the fatigue strength can be reduced. Loads that previously posed no problem can then contribute to further damage. The design S-N curves help to take this effect into account.
CorrosionAs corrosion increases, the fatigue strength
of a component decreases. It promotes the initiation and
growth of cracks.
Notch effectThe sharper the notch, the more negative the influence on the fatigue strength of the component. On the other hand, the fatigue strength with respect to the local notch stress increases due to the supporting effect.
TemperatureAt low temperatures, static strength increases and, as a rule, so does fatigue strength. However, ductility decreases, which in turn has a negative effect on fatigue strength. At high temperatures, on the other hand, fatigue strength
decreases. Exactly when this happens varies depending on the material.
The FKM guideline provides for temperature to be taken into account outside the following ranges:
● Steel: -40 °C to 500 °C
● Cast iron: -25 °C to 500 °C
● Aluminium: -25 °C to 200 °C

How can fatigue strength be increased?

The main levers for increasing the fatigue strength of a component are the design of the machine and surface hardening of the material. If the design achieves a lower notch effect, fatigue strength automatically increases as a result. To increase the fatigue strength of the material itself, surface hardening by means of edge layer hardening or case hardening is suitable.

Related glossary entries