What are residual stresses?
Residual stresses result from uneven expansion and contraction that occur during the manufacture or processing of metal parts. A common example is uneven cooling after welding, which can lead to local expansion and thus to residual stresses.
In principle, every component has residual stresses. Depending on their magnitude, they can cause slight distortion but also severe deformation. The metal also becomes more susceptible to material fatigue and cracking. It is therefore important to minimise residual stresses through suitable manufacturing techniques and post-treatment processes such as stress-relief annealing.
Classification of residual stresses
There are two different approaches to classifying residual stresses – by extent and by time course.
1 Classification by extent
When residual stresses are classified by their extent, the actual distribution of the stresses in the material is considered.
Macroscopic residual stresses (type I)
Macroscopic stresses are visible to the naked eye or by simple measuring methods. They extend over several grains and are often distributed over the entire component or large parts of it. They therefore have a major influence on the properties of the component. Typical causes are welding, casting and uneven cooling processes.
Microscopic residual stresses (type II)
Microscopic residual stresses extend over one grain and are the result of
irregularities in the crystal structure, such as dislocations, grain boundaries or
different phases. They influence properties such as the ductility and
the fracture toughness of a metal.
Submicroscopic
residual stresses/nano residual stresses (type III)
Submicroscopic stresses occur within a small region of a grain . They are caused by defects and dislocations at the atomic level. Because of their small extent, they have only a limited influence on the mechanical properties of a component, but can influence processes such as diffusion at the atomic level.

2 Classification by time course
Classification by time course focuses on when the residual stresses occur and how long they remain in the material.
Temporary stresses
Temporary stresses are present in a material only for a limited time and disappear once the cause is removed or when the material has adapted to the new situation. They occur, for example, with uneven cooling.
Latent stresses
If temporary stresses exceed the yield strength, latent stresses arise, which can be eliminated by measures such as stress-relief annealing or annealing.
Permanent stresses
Permanent stresses arise from inhomogeneous thermal expansion during cooling. They can be relieved not only by annealing but also by mechanical working and machining processes.
Causes and effects of residual stresses in materials and components
Residual stresses can have many different causes, which can be categorised in different ways.
Plastic deformation
| Cold forming | – Residual stresses arise from different expansions and deformations in different areas of the material – typical for bending, drawing or rolling |
| Mechanical machining | – Residual stresses arise from local plastic deformation at or near the surface – typical for milling, drilling or grinding |
Inhomogeneous structural transformation
| Phase transformation | – uneven changes in the structure generate residual stresses – typical for welding and heat treatments – e.g. volume change due to martensitic transformation |
| Casting | – Residual stresses arise from different shrinkage due to uneven cooling, because the edge cools faster than the core |
Thermal influences
| Local heating | – only a certain area of the component is heated, which leads to stresses – typical for welding |
| Temperature gradient | – Residual stresses due to uneven temperature distribution in the material during heating or cooling |
Other causes of residual stresses
There are also a number of other causes of residual stresses, which can result from the material properties or from the geometry of the component – for example a high coefficient of expansion and anisotropic properties, or complex geometries, sharp edges and uneven cross-sections.
How can I measure residual stresses?
Residual stresses can be measured using destructive, semi-destructive and non-destructive methods. Which technique is used depends on the available resources and the desired depth of information.
Destructive testing
In destructive testing, the object being measured is destroyed. This can be useful in development, for example. Destructive tests are comparatively inexpensive. Typical examples are the contour method and slitting.
In the contour method, the sample is separated into two parts. This technique provides a 2D map of the residual stresses perpendicular to the measurement plane across the entire material cross-section.
In the slitting method, the workpiece is cut deeply. The deformations are then measured as a function of the slit depth. From the results, through-thickness residual stresses perpendicular to the cut can be calculated.
Semi-destructive testing
In semi-destructive tests, only small amounts of material are removed. Apart from that, the basic principle is comparable to destructive testing. Examples are deep-hole drilling and centre-hole drilling.
In deep-hole drilling, a hole is first drilled through the sample and then a circular core of material is cut out around the hole. The residual stresses can be calculated from the geometric changes between the diameter of the first hole and that of the second hole.
Centre-hole drilling is a method for measuring deformations around the drilled hole. Strain gauges are used for this. The residual stresses can be calculated from the results.
Non-destructive testing
Non-destructive tests make it possible to measure residual stresses and assess structural integrity while the object remains intact and can continue to be used. Various methods are available for this.
Neutron diffraction uses neutrons to measure the crystal lattice spacing. Going further, a synchrotron can be used to accelerate the electromagnetic radiation. In addition, X-ray diffraction allows surface residual stresses to be measured.
Reducing residual stresses: heat treatment processes for stress reduction
To prepare a component optimally for its intended use and to ensure reliability in operation, residual stresses in the material must be minimised. HÄRTHA GROUP offers the following processes for this:
- Stress-relief annealing: Stress-relief annealing takes place below the individual transformation temperature of the material concerned and is regarded as a very effective heat treatment for reducing residual stresses.
- Normalising: In normalising, the steel is heated to a temperature above its transformation temperature and then cooled in gas or in air. This reduces hardness, tensile strength and residual stresses in the material at the same time.
- Tempering: The tempering temperature is material-specific and can be taken from so-called material data sheets. Tempering makes it possible to set the desired final hardness of a component. Slow cooling then follows. This reduces hardness, tensile strength and residual stresses,
while toughness increases. Depending on the material or steel grade, multiple tempering cycles may be required.
Positive and negative effects of residual stresses
High residual stresses are undesirable and should be reduced, but residual stresses can also have positive effects on a material and are deliberately used to achieve, for example, the following properties:
- Increased strength: Compressive residual stresses can increase the strength of components, e.g. in pressure vessels or turbines.
- Higher corrosion resistance: Residual stresses can have a positive influence on corrosion resistance, e.g. in pipelines or fittings.
- Higher load capacity: Residual stresses can give components higher fatigue strength, e.g. springs and axles.
- Optimised deformation behaviour: Residual stresses influence the deformation behaviour of metals. This is relevant, for example, for forming tools or a wide variety of sheet metal parts.
However, even deliberately introduced residual stresses must be controlled in order to avoid problems such as cracking in welded structures, a lack of dimensional accuracy in
precision components, or material failure in vehicles or structures.
Conclusion
Only when residual stresses are optimally adjusted can components achieve the desired properties such as smooth deformation behaviour, high strength or low brittleness. In addition to in-depth technical knowledge, this requires a great deal of experience
on the part of the specialists who work the metal.