Ferritic steel

Updated on: 11.11.2024

Ferritic steel is a special group of stainless steels with a chromium content of 10.5 to 27 %. The iron-rich body-centred cubic crystal structure of ferrite gives these steel grades strong magnetic properties. The carbon content is below 0.20 %. Depending on the composition, alternative names such as chromium steel, chromium-nickel steel or chromium stainless steel are also common.

Characteristic properties

The high chromium content of ferritic steels has a positive effect on corrosion resistance to water, air, acids and alkalis. Molybdenum can increase this resistance further. As a result, these steel grades also withstand particularly harsh conditions and aggressive environments.

 

The low carbon content also contributes to the corrosion resistance of ferritic steels. However, it also reduces ductility and therefore formability. Even so, ferritic steel is suitable for cold forming. The low carbon content and the high chromium content produce a temperature-stable microstructure that cannot be hardened further by heat treatment.

Ferritic steel vs. austenitic steel

In contrast to austenitic steels, the nickel content of ferritic steels is low or absent. Properties such as ductility and toughness are achieved by the chromium-iron alloy, but are lower than in austenitic steels. Here are the most important characteristics in comparison:

 

  • Magnetism: Unlike austenitic steels, the body-centred cubic lattice structure gives ferritic steel strong magnetic properties.
  • Strength: Ferritic steel offers higher strength than austenitic steel, especially after cold working.
  • Weight: Ferritic steels can be lighter than austenitic steels.
  • Weldability: Ferritic steels are harder to weld than austenitic steels. However, adding niobium or titanium can improve weldability.
  • Density: Ferritic steels have a density between 7.7 and 8.0 g/cm³. Austenitic steels are at 7.9 to 8.0 g/cm³.
  • Price: Because they contain little or no nickel, ferritic steels are cheaper than austenitic steels.
  • Recycling: Like most metals, ferritic steels can be recycled well.

Applications

Ferritic steel is used in a wide variety of applications that make use of its specific properties. Here are some of the most common fields of use:

 

  • Automotive industry: Exhaust systems, bodywork, catalytic converter housings, etc.
  • Household appliances: Hotplates, dishwasher and refrigerator parts and other components
  • Construction: Railings, door frames, façade cladding, roofing, pipework and other structural elements
  • Chemical industry: Fittings, pipework and tanks that come into contact with aggressive media
  • Food industry: Processing plants, kitchen accessories and other applications

Different types of ferritic steel grades

Depending on their properties and field of application, the various ferritic steel grades can be divided into five commonly used groups. There are also other ferritic steel grades beyond these.

GroupDescription and applications
Group 1 (type 409, 410, 410L, 420)• Lowest-cost stainless steel grades
• Chromium content up to 14 %
• Application examples: catalytic converter housings, LCD monitor frames, containers, buses
Group 2 (type 430)• Most widely used ferritic steel grade worldwide
• Chromium content between 16% and 18%
• Better corrosion resistance than group 1
• Application examples: washing machine drums, kitchen sinks, pots, pans, knife blades
Group 3 (type 430TI, 439, 441)• Chromium content between 17.5% and 18.5%
• Alloying additions such as titanium and niobium provide better weldability and formability
• Application examples: exhaust systems, kitchen sinks
Group 4 (type 434, 436, 444)• Increased corrosion resistance thanks to molybdenum
• Fields of application: corrosive environments, hot water tanks, outdoor applications
Group 5 (type 446, 445)• Very high corrosion resistance (comparable to titanium steel) thanks to a high chromium and molybdenum content
• Application examples: heat exchangers, water heaters, boilers

Hardening of ferritic steel grades

Heat treatments such as hardening and tempering cannot increase the hardness of ferritic steels, because the crystalline ferrite structure does not transform when heat is applied. To achieve higher density, strength and hardness, however, the microstructure can be influenced by cold forming such as forging, rolling or drawing.

 

Heat treatments are nevertheless useful for optimising other properties of ferritic steels:

 

  • Annealing relieves stresses in the material at temperatures between 500 °C and 700 °C and thus increases the ductility and toughness of ferritic steels.
  • Normalising is carried out at higher temperatures than annealing. The aim is a finer grain size and more uniform material properties.

 

In addition, chemical-physical surface hardening processes such as a Tenifer treatment or nitriding can improve the hardness, wear resistance and corrosion resistance of the surface of ferritic steels.

Related glossary entries